INTRODUCTION
High Strength

Good Insulation

Good Heat Resistance

High Strength Retention Rate

| Properties | Test Standard | Unit | Typical Value |
| Fiberglass Content | GB/T 15568-2008 | wt% | 48±3 |
| Moulding Temperature | / | ℃ | 130-150 |
| Moulding Pressure | / | Mpa | 7-10 |
| Shrinkage | / | % | ≤0.05 |
| Density | GB/T 1463-2005 | g/cm3 | ≤1.90 |
| Tensile Strength | GB/T 1447-2005 | MPa | ≥150 |
| Flexural Strength | GB/T 1449-2005 | Mpa | ≥280 |
| Flexural Modulus | GB/T 1449-2005 | GPa | ≥12 |
| Impact Strength | GB/T 1451-2005 | KJ/m2 | ≥100 |
| After 180℃*1000H Check the tensile and bending strength on the side | Strength Retention Rate | % | ≥70 |
| Heat-Resisting Derofmation Temperature | GB/T 1634-2004 | ℃ | ≥240 |
| Flame Retardant Rating | UL-94 | / | V0@3mm |